Product Feature
1.Advanced machining processing technique: Solid-Liquid machining processing technique to bond copper and aluminum in oxygen-free environment permanently and firmly. Also, the combination strength continues to reinforce when use.
Product Specification/Models
Thickness 0.5-15mm
Width small than 1000mm
Length As request
Application
1.Electric power industry (conductive industry)2. Decoration industry3. Shipping industry4. Heat conduction industry 5. The auto industry6. Air conditioning radiator
Specification(thickness * width): 0.1-15mm * 30-2000mm
Cooper and Aluminum weight ratio: Cu:AL 32%-40%: 60%-68%
Cooper and Aluminum volume ratio: Cu:AL 15-20: 80-85
Density(g/cm3):3.5-3.9
Resistivity(mm2/m): little than 0.019
Tensile Strength(N/mm2):more than 120
Elongation (%):27-30
Peeling Strength(N/mm): more than 12
Best quality aluminum copper composite panels